Metal protective coatings
EpoMor D27E Economy High-Build Intermediate Coat
For steelwork projects considering an intermediate coat to build film thickness.
EpoMor D27E · Intermediate layer
Key specifications
| Product role | Economy epoxy intermediate coat |
|---|---|
| Chemistry | Epoxy |
| Components | Two components (2K) |
| Dry film thickness | 60–80 µm per coat. |
| Theoretical coverage | 8.5–11.3 m²/L at the stated DFT, before thinning and site losses. |
| Mix ratio A:B | 9:1 by weight |
| Colour | Standard / RAL on request |
| Volume solids | 68.0% by volume (66.0%–70.0%) |
| Mass solids | 81.0% by weight (79.0%–83.0%) |
| Density | 1.450 kg/L at 25 °C, mixed A+B before thinning |
Additional engineering and product references
- VOC content
- <420 g/L
- Wet film thickness
- 88–118 µm per coat before thinning.
TDS & SDS
TDS Technical data sheet
A Component SDS
B Component SDS
Coating system
Use the full EpoMor D27E name. List the primer and finish under consideration; do not assume compatibility with EpoPri D27E.
- Confirm film build and compatibility with both adjacent coats. This is not EpoPri D27E, and historical values are not validated by the epoxy identity.
When a steel intermediate coat is used
For structural steel: compare atmospheric exposure categories C1–C5
Substrate preparation
Identify the specified primer or preceding coat. Check its condition, cleanliness and recoat window before applying this intermediate coat; confirm what correction is needed if that window was missed.
For structural steel, use these checks:
Application reference
| Application method | Brush / roller / spray |
|---|---|
| Application temperature | 10–30 °C |
| Relative humidity | ≤80% |
| Mix ratio A:B | 9:1 by weight |
| Pot life | Engineering working time: maximum 4 h at 25 °C. Start timing when A and B are first combined; induction and application are included. Discard material when this time expires or when application viscosity rises, whichever occurs first. |
| Touch dry | ≤1 h at 25 °C |
| Hard dry | 4 h at 25 °C |
| Recoat interval | 6 h–72 h at 25 °C; after maximum, clean and abrade before recoating. |
| Full cure | 7 days at 25 °C |
| Thinner | EpoThi 20 |
| Thinning reference | Use EpoThi 20, 0–10% by volume of the mixed coating, for all permitted methods. Thinner supply density: ≤1.00 kg/L at 25 °C. |
Packaging & ordering
| Packaging | Use the product-specific matched kit listed under Component packaging. Identify the net mass of each component on its label. |
|---|---|
| Matched component set | A 18 kg + B 2 kg / 20 kg set |
| Shelf life | 12 months |
Include the quantity, delivery country and colour reference in your enquiry.