Metal protective coatings
EpoMor D24 High-Build Epoxy Barrier Intermediate Coat
For steel projects where an intermediate coating layer is being specified.
EpoMor D24 · Intermediate layer
- Finish coat
- EpoMor D24 · Intermediate coat
- Primer
- Prepared steel plate
Key specifications
| Product role | High-build intermediate coat |
|---|---|
| Chemistry | Epoxy |
| Components | Two components (2K) |
| Dry film thickness | 150–200 µm per coat. |
| Theoretical coverage | 4.0–5.3 m²/L at the stated DFT, before thinning and site losses. |
| Mix ratio A:B | 10:1 by weight |
| Colour | Standard / RAL on request |
| Volume solids | 80.0% by volume (78.0%–82.0%) |
| Mass solids | 87.0% by weight (85.0%–89.0%) |
| Density | 1.400 kg/L at 25 °C, mixed A+B before thinning |
Additional engineering and product references
- VOC content
- <420 g/L
- Wet film thickness
- 188–250 µm per coat before thinning.
TDS & SDS
TDS Technical data sheet
A Component SDS
B Component SDS
Coating system
Use the full EpoMor D24 name and confirm the existing primer, target build-up and proposed finish.
- Confirm per-coat thickness and whether the build requires more than one coat. EpoPri D24 is a different product.
When a steel intermediate coat is used
For structural steel: compare atmospheric exposure categories C1–C5
Substrate preparation
Identify the specified primer or preceding coat. Check its condition, cleanliness and recoat window before applying this intermediate coat; confirm what correction is needed if that window was missed.
For structural steel, use these checks:
Application reference
| Application method | Mainly airless spray |
|---|---|
| Application temperature | 10–35 °C; maintain the air, coating and substrate at ≥10 °C during application and drying. |
| Relative humidity | ≤80% during application and drying. |
| Mix ratio A:B | 10:1 by weight |
| Pot life | Engineering working time: maximum 1 h at 25 °C. Start timing when A and B are first combined; induction and application are included. Discard material when this time expires or when application viscosity rises, whichever occurs first. |
| Touch dry | ≤3 h at 25 °C |
| Hard dry | Engineering through-dry control: inspect after 24 h at 25 °C at 150 µm and 200 µm DFT; record the defined dry-through result and confirm a firm, clean film before recoating. |
| Recoat interval | Minimum 24 h at 25 °C for 150–200 µm DFT per coat; verify a firm, dry, clean surface before recoating. Maximum 7 days; after this, clean and abrade. |
| Full cure | 7 days at 25 °C |
| Thinner | EpoThi 10 |
| Thinning reference | Use EpoThi 10, 0–4% by volume of the mixed coating, for all permitted methods. Thinner supply density: ≤1.00 kg/L at 25 °C. |
Packaging & ordering
| Packaging | Use the product-specific matched kit listed under Component packaging. Identify the net mass of each component on its label. |
|---|---|
| Matched component set | A 20 kg + B 2 kg / 22 kg set |
| Shelf life | 12 months |
Include the quantity, delivery country and colour reference in your enquiry.
LET’S TALK MATERIALS
Your project.
A clearer next step.
Tell us what you know. Leave the technical unknowns to the conversation.